Thermal Properties Metric English Comments
Melting Point 47.0 - 49.0 °C
117 - 120 °F
Hong Kun Group BP 12 Additive
Chemical Name: 2-hydroxy-4-(octyloxy)benzophenoneCAS No. 1843-05-6All information provided by Hongkun Group
Melting Point 47.0 - 49.0 °C
117 - 120 °F
Hong Kun Group UV 531 UV Absorber
Chemical Name: 2-hydroxy-4-(octyloxy)benzophenoneCAS No. 1843-05-6All information provided by Hongkun Group
Melting Point 47.0 - 49.0 °C
117 - 120 °F
M Chemical GUARD DOGâ„¢ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative
GUARD DOGâ„¢ UV531(flake or powder) light stabilizer is a derivative of Benzophenone that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - ..
Melting Point 47.0 - 52.0 °C
117 - 126 °F
Indium Corp. Indalloy 16 Low Melting Bismuth Alloy
Information Provided by Indium Corporation
Melting Point 47.0 °C
117 °F
Eutectic
Indium Corp. Indalloy® 117 Bi-Pb-In-Sn-Cd Fusible Alloy
General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation.
Melting Point 47.0 - 57.0 °C
117 - 135 °F
Struktol V-DSP Processing Additive
Fatty acid esterTypical Applications: STRUKTOL® V-DSP is a highly compatible, internal PVC lubricant. It is particularly good at improving melt flow thus reducing amperage and head pressure for c..
Melting Point 47.0 - 49.0 °C
117 - 120 °F
Suqian Unitechem UV-531
Chemical Name: 2-Hydroxy-4-Octyloxy BenxophenoneCAS NO.: 1843-05-6Properties: Freely soluble in benzene, n-hexane, acetone, slightly soluble in ethanol, very slightly soluble in ethane dichloride.Us..
Melting Point 47.0 - 88.0 °C
117 - 190 °F
ASTM D3418(DSC)
DuPont Surlyn® 8945 Thermoplastic Ionomer Resin
Surlyn® 8945 provides high flow properties and consistent, easy processing in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer sp..
Melting Point 47.0 °C
117 °F
AIM 47 Fusible Bismuth Alloy
Uses: low-temperature solder; fixturing delicate parts for machining; lens blocking; proof casting of cavities; dental models; fusible element in safety devices and alarms; radiation blocking for x-..
Melting Point 47.0 - 105 °C
117 - 221 °F
Average value: 84.7 °C Grade Count:40
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..
Melting Point 47.0 °C
117 °F
Freezing Point; ASTM D3418
DuPont Elvax® CM576 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® CM576 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low ..
Melting Point 47.0 °C
117 °F
Freezing Point; ASTM D3418
DuPont Elvax® CM4875 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® CM4875 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low..