Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 200 - 240 °C | 392 - 464 °F | Average value: 222 °C Grade Count:30 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Melting Point | 221 - 240 °C | 430 - 464 °F | |
Indium Corp. Indalloy 132 Tin Solder Alloy High temperature electrical solderInformation Provided by Indium Corporation |
|||
Melting Point | 235 - 240 °C | 455 - 464 °F | |
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â.. |
|||
Melting Point | 232 - 240 °C | 450 - 464 °F | |
Williams Advanced Alloys WS240 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |