Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 231 - 330 °C | 448 - 626 °F | |
Indium Corp. Indalloy 172 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | <= 231 °C | <= 448 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 102.LC Low Density Polyethylene Resin Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawn down to thing gauges.Availability: Latin America, North America and S.. |
|||
Melting Point | <= 231 °C | <= 448 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LGA 105 Low Density Polyethylene Resin Product Description: LGA 105 is a homopolymer, garment film resin with good toughness. It is capable of being draw-down to thin gauges.Availability: North America Additive: Antiblock: NoSlip: NoPro.. |
|||
Melting Point | 231 °C | 448 °F | ASTM D3418 |
Ashley Polymers Ashlene® 559LD-33G Nylon 66, 33% Glass Reinforced A high impact reinforced nylon copolymer with good low temperature properties.Data provided by the manufacturer |
|||
Melting Point | 231 °C | 448 °F | ASTM D3418 |
Ashley Polymers Ashlene® 727 Nylon 6 A modified nylon for applications requiring flexibility.Data provided by the manufacturer |