Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 325 - 330 °C | 617 - 626 °F | ISO.3146 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Melting Point | 325 - 330 °C | 617 - 626 °F | ISO.3146 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ISO 11357-3 |
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melting Point | 325 - 330 °C | 617 - 626 °F | |
Solvay Specialty Polymers Polymist® F-5A EX PTFE Powder Lubricant
(Unverified Data**) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Melting Point | 325 - 330 °C | 617 - 626 °F | |
Solvay Specialty Polymers Polymist® F-510 PTFE Powder Lubricant
(discontinued **) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Melting Point | 327 - 330 °C | 621 - 626 °F | Average value: 327 °C Grade Count:11 |
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma.. |
|||
Melting Point | 231 - 330 °C | 448 - 626 °F | |
Indium Corp. Indalloy 172 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | DSC |
Solvay Specialty Polymers Algoflon® L100 Polytetrafluoroethylene (PTFE) Algoflon® L100 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L100 can be de-agglomerated.. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L600 Polytetrafluoroethylene (PTFE) Algoflon® L600 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L600 can be de-agglomerated.. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro FR-150 Anti-dripping Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins (and to polymeric resins containing glass fiber) provides greatly increased resistance to surface wear and abrasi.. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 607 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 615 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 702 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 707 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 715 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 802 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 803 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 807 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 811 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 815 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies MicroFLON® 1253 Thermoplastic Grade PTFE Additive Special grade for fine dispersion.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a.. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 602 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 603 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 611 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |