Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 727 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 727 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A modified nylon for applications requiring flexibility.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ATSM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Modulus 0.970 GPa
141 ksi
ASTM D790
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 231 °C
448 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C
109 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved