Thermal Properties Metric English Comments
Melting Point 220 - 222 °C
428 - 432 °F
DSC @ 15°C/min; ASTM D3418
Ovation Polymers Opnyl OP6MT254 Nylon 6
Nylon 6 – Mighty Tough plasticized extrusion grade for tubing/profile applications. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are p..
Melting Point 183 - 222 °C
361 - 432 °F
Indium Corp. Indalloy 122 Tin-Lead Solder Alloy
Information Provided by Indium Corporation