Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 307 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 153 °C
307 °F
Indium Corp. Indalloy 91 Indium Solder Alloy
Information Provided by Indium Corporation
Melting Point 153 °C
307 °F
DSC
Total PPH M3382MZ Homopolymer Polypropylene, Clarified Metallocene Sheet Extrusion and Thermoforming Resin
Clarity. TOTAL Polypropylene M3382MZ produces thermoformed parts with superior clarity, gloss and excellent side wall stiffness.Recommended Applications. TOTAL Polypropylene M3382MZ is ideal for d..
Copyright © lookpolymers.com All Rights Reserved