Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 96.0 - 143 °C | 205 - 289 °F | |
Indium Corp. Indalloy 85 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 110 - 143 °C | 230 - 289 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN .. |
|||
Melting Point | -75.0 - 143 °C | -103 - 289 °F | Average value: 74.6 °C Grade Count:34 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |