Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -75.0 °C | -103 °F | Freezing Point |
LG Chemical Ethyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |
|||
Melting Point | -75.0 °C | -103 °F | Freezing Point |
LG Chemical Methyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |
|||
Melting Point | <= -75.0 °C | <= -103 °F | |
BASF N-Ethylpyrrolidone-2 (NEP) Formula: C6H11NOCAS: 2687-91-4Description: N-Ethylpyrrolidone-2 (NEP) Is a colorless to yellow liquid, with an amine like odor. It is miscible in water and soluble in other organic solvents.Synonym.. |
|||
Melting Point | <= -75.0 °C | <= -103 °F | |
BASF 2-Ethylhexanoyl Chloride Formula: C8H15ClOCAS: 760-67-8Description: 2-Ethylhexanoyl chloride is a colorless to yellowish liquid with a pungent odor. It is miscible with all common organic solvents. It hydrolyses in the pres.. |
|||
Melting Point | -75.0 °C | -103 °F | Freezing Point |
BASF Methyl Acrylate Formula: C4H6O2CAS: 96-33-3Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Methyl acrylate forms homopolymers and copolymers. Copolymer.. |
|||
Melting Point | -75.0 - 143 °C | -103 - 289 °F | Average value: 74.6 °C Grade Count:34 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |