Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 96.0 °C | 205 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 1302 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
(discontinued **) 13 wt% Methacrylic Acid.Nucrel® 1302 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process po.. |
|||
Melting Point | 96.0 °C | 205 °F | Exxon Method |
ExxonMobil Escorene® LD-701 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10.5% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughnes.. |
|||
Melting Point | 96.0 °C | 205 °F | Exxon Method |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Melting Point | 96.0 °C | 205 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® NWL Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® NWL is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Film produced from this resin is .. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3418 |
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melting Point | 96.0 °C | 205 °F | |
LG Chemical LC100 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear applicationApplication: Polymer modification, Shoe sole, Film coex.. |
|||
Melting Point | 96.0 - 180 °C | 205 - 356 °F | |
Indium Corp. Indalloy 105 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 - 137 °C | 205 - 279 °F | |
Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 - 139 °C | 205 - 282 °F | |
Indium Corp. Indalloy 83 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 - 143 °C | 205 - 289 °F | |
Indium Corp. Indalloy 85 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 °C | 205 °F | Eutectic |
Indium Corp. Indalloy® 42 Bi-Sn-Pb Solder Alloy Bismuth added to achieve a low melting point. Fair wettability.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 96.0 °C | 205 °F | ISO 3146 |
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h.. |
|||
Melting Point | 96.0 °C | 205 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also.. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3417- ISO 3146 |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |
|||
Melting Point | 96.0 °C | 205 °F | TRN-14 |
Tipco Tipcolite® TPF 1115 - Unreinforced Thermoset Phenolic Resin, 43 mm Norton Flow with 9% Hexamine Unreinforced Phenolic Resin having 43mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: BrakeliningInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Melting Point | 96.0 °C | 205 °F | by DSC; ASTM D3418 |
Westlake EMAC® Plus SP1305 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1305 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1305 is.. |
|||
Melting Point | 96.0 °C | 205 °F | DSC; ASTM D3418 |
Westlake Tymax™ GA7501 Anhydride Modified Acrylate Copolymer (Developmental) Westlake GA7501 is an anhydride modified acrylate copolymer for extrusion coating and cast film tie-layers. This resin is designed to function as a coextruded tie-layer in multilayer applications wh.. |
|||
Melting Point | 96.0 °C | 205 °F | DSC; ASTM D3418 |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 96.0 °C | 205 °F | DTA |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 96.0 °C | 205 °F | Dow Method (DSC) |
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre.. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2910 M Q 47 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2920 M Ethylene/Acrylate Copolymer Used in the manufacture of economical composite films of Lucalen and PE-LD, and as a primer for aluminum steel composites.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2920 M Q 225 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | 10°C/min |
Arkema Group Evatane® 1090 VN 3 Ethylene Vinyl Acetate Description: EVA copolymer made by high pressure tubular process.Applications:Grade for molding flexible articles.Examples: Closures, plugs, swimming flippers, toys.ISO data provided by the manufact.. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2910 M Ethylene/Acrylate Copolymer For coating metals such as aluminum and steel, and as a primer for composites of metal or paper with Lupolen. Contains an antioxidant.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 96.0 °C | 205 °F | Eutectic |
Indium Corp. Indalloy 39 Bismuth Solder Alloy Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation |
|||
Melting Point | 96.0 °C | 205 °F | ISO 3146 |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |