Polymer Property : Melting Point = 278 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 278 - 280 °C
532 - 536 °F
Average value: 280 °C Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Melting Point 278 °C
532 °F
ASTM D789
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin
Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit..
Melting Point 278 °C
532 °F
ASTM D789
E-Polymers SEPAZ® K115HF 15% Glass Fiber Reinforced High Flow PPS Resin
Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit..
Melting Point 278 °C
532 °F
ASTM D789
E-Polymers SEPAZ® K130HF 30% Glass Fiber Reinforced High Flow PPS Resin
Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit..
Melting Point 278 - 285 °C
532 - 545 °F
Average value: 282 °C Grade Count:29
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..