Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 253 - 257 °C | 487 - 495 °F | QCD--W1-49 |
Pearl Engineering PEPLPET D-101-SH Monofilament Resin Used in the paper industry as paper pulp nets. |
|||
Melting Point | 253 - 257 °C | 487 - 495 °F | QCD--W1-49 |
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |
|||
Melting Point | 115 - 257 °C | 239 - 495 °F | ASTM D3418 |
3M Dyneon™ THV™ 200P Fluorothermoplastic, Powder Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Melting Point | 115 - 257 °C | 239 - 495 °F | ASTM D3418 |
3M Dyneon™ THV™ 200G Fluorothermoplastic, Pellet Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Melting Point | 183 - 257 °C | 361 - 495 °F | |
Indium Corp. Indalloy 141 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 257 °C | 361 - 495 °F | |
Williams Advanced Alloys WS257 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |