Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 221 - 254 °C | 430 - 489 °F | Average value: 226 °C Grade Count:20 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Melting Point | 135 - 254 °C | 275 - 489 °F | Average value: 237 °C Grade Count:17 |
Overview of materials for Nylon 66 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66 Fiber". Each property range of values reported is minimum and maximum values of appropriate Mat.. |