Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 165 - 203 °C | 329 - 397 °F | Average value: 168 °C Grade Count:32 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Melting Point | 193 - 203 °C | 379 - 397 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® 11T98 Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T98 is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, combining high hardness with excellent mechanical properties. It can be extruded.. |