Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 950 °C | 1740 °F | Eutectic |
Indium Corp. Indalloy 196 Gold Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 949 - 1070 °C | 1740 - 1950 °F | |
Universal Wire Works BNi-1A (AMS 4776) Nickel Base Brazing Filler Metal Low Carbon (compare to BNi-1)Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Melting Point | 950 °C | 1740 °F | |
Goodfellow Nioro® Gold 82/Nickel 18 Alloy Brazing alloy. Melting point 950C. Good corrosion resistance in oxidizing conditions.Information provided by Goodfellow. |