Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 179 - 189 °C | 354 - 372 °F | |
Indium Corp. Indalloy 137 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 177 - 189 °C | 351 - 372 °F | |
Johnson Matthey JM6236 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 183 - 189 °C | 361 - 372 °F | |
Williams Advanced Alloys WS199 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |