Polymer Property : Melting Point = 178 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 165 - 178 °C
329 - 352 °F
Average value: 170 °C Grade Count:32
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Melting Point 175 - 178 °C
347 - 352 °F
Average value: 178 °C Grade Count:7
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Melting Point 175 - 178 °C
347 - 352 °F
Average value: 177 °C Grade Count:5
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..
Melting Point 174 - 178 °C
345 - 352 °F
Average value: 175 °C Grade Count:5
Overview of materials for Nylon 12, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr..
Melting Point 168 - 178 °C
334 - 352 °F
Average value: 174 °C Grade Count:14
Overview of materials for Nylon 12, Extrusion/Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values ..
Melting Point 174 - 178 °C
345 - 352 °F
Average value: 175 °C Grade Count:6
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Melting Point 165 - 178 °C
329 - 352 °F
DIN 53736
Isoflon PVDF Polyvinylidene fluoride
Electrical and thermal insulating products with food slipping propertiesChemically inertInformation provided by Isoflon.