Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 166 °C | 330 °F | ASTM D3418 |
Custom Resins Duratel™ MF3 Acetal Copolymer
(discontinued **) Description: Duratel™ MF3 is a 2.5 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Melting Point | 166 °C | 330 °F | ASTM D3418 |
Custom Resins Duratel™ MF13 Acetal Copolymer
(discontinued **) Description: Duratel™ MF13 is a 13 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Melting Point | 166 °C | 330 °F | ASTM D3418 |
Custom Resins Duratel™ MF27 Acetal Copolymer
(discontinued **) Description: Duratel™ MF27 is a 27 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Melting Point | 166 °C | 330 °F | DSC |
M. Holland Company PP720 Polypropylene Homopolymer Gas-fading resistantHomopolymerGood processabilityGood UV resistanceApplications: FabricsSpunbond non-wovensYarn |
|||
Melting Point | 166 - 174 °C | 330 - 345 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Melting Point | 166 °C | 330 °F | |
Techmer ES HiFill® POM CO GC20 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Melting Point | 166 °C | 330 °F | ASTM D4591 |
Westlake Plastics Clariflex® TFE/VF2/HFP Clariflex is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoro-propylene, and vinylidene fluoride. Notable properties include light transmission, chemical resistance.. |
|||
Melting Point | 166 °C | 330 °F | ASTM D4591 |
Westlake Plastics Propylux® Polypropylene Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance it abrasion. These properties makes it suitable f.. |
|||
Melting Point | 166 °C | 330 °F | ASTM D3418 |
Ensinger TECAFINE™ PP Polypropylene (PP) TECAFINE™ PP is an anti-stated, polypropylene, random copolymer polyolefin engineering plastic providing excellent chemical resistance and high purity. FDA compliant with better mechanical propert.. |
|||
Melting Point | 166 °C | 330 °F | |
Techmer ES Statiblend® PP CO 99074 Availability: North AmericaForms: PelletsFeature: Copolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Melting Point | 166 °C | 330 °F | ASTM D3417 |
Quantum Polycarbonate 20% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Melting Point | 166 °C | 330 °F | ASTM D3418 |
Custom Resins Duratel™ MF9 Acetal Copolymer
(discontinued **) Description: Duratel™ MF9 is a 9 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |