Polymer Property : Melting Point = 160 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 71.1 °C
160 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® LD 767.MJ Blown Film Resin  (discontinued **)
Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical
Melting Point 71.1 °C
160 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin  (discontinued **)
Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical
Melting Point 71.0 - 74.0 °C
160 - 165 °F
Hong Kun Group DETX Additive
CAS No. 82799-44-8All information provided by Hongkun Group
Melting Point 71.0 - 93.0 °C
160 - 199 °F
TMA Melt Range
Huntsman IROGRAN® CA 117-200 DP TPU-Polyester
Polyester-based TPUs that are specially designed for adhesives applications where high green strength and a fast crystallization rate are essential qualities.Information provided by Alliance Polymer..
Melting Point 71.0 - 88.0 °C
160 - 190 °F
TMA Melt Range
Huntsman IROGRAN® PS 456-202 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Melting Point 71.0 °C
160 °F
DSC; ASTM D3418
ICO Polymers ICOFLOâ„¢ 510-5004 1000 Micron EVA Powder
Description: ICOFLO 510-5004 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste..
Melting Point 71.0 °C
160 °F
DSC; ASTM D3418
ICO Polymers ICOTEXâ„¢ 520-5004 1000 Micron EVA Powder
Description: ICOTEX 520-5004 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and flexibility and a viny..
Melting Point 71.0 - 88.0 °C
160 - 190 °F
Indium Corp. Indalloy 160-190 Fusible Bismuth Alloy
Information Provided by Indium Corporation
Melting Point 71.0 °C
160 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
15 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Melting Point 71.1 °C
160 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® UL 8705 Adhesive Application Resin
Escorene Ultra UL 8705 is a relatively low viscosity, 27.6% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has ..
Melting Point 71.1 °C
160 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® UL 8705E Adhesive Application Resin
Escorene Ultra UL 8705 is a relatively low viscosity, 29% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has go..
Melting Point 71.0 °C
160 °F
ASTM D3418, ISO 3146
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate
Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a ..
Melting Point 71.0 °C
160 °F
ASTM D3418, ISO 3146
DuPont™ Fusabond® C190 Polymer Modifier
DuPont™ Fusabond® C190 is a anhydride modified ethylene vinyl acetate copolymer. Uses: Adhesives Pipe Coating Polymer Modifier
Melting Point 71.0 °C
160 °F
ASTM D3418, ISO 3146
DuPont™ Fusabond® C250 Polymer Modifier
DuPont™ Fusabond® C250 is a modified ethylene vinyl acetate copolymer. Used as an adhesion promoter and coupling agent.
Melting Point 71.0 °C
160 °F
DSC
Arkema Group EVATANE® 28-25 Copolymer Ethylene - Vinyl Acetate
EVATANE® 28-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-25 is stabilized with antioxidants. The High Vinyl Acetate co..
Melting Point 71.0 °C
160 °F
Upon Melting via DSC/ASTM D3418
DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process ..
Melting Point 71.0 - 225 °C
160 - 437 °F
Average value: 155 °C Grade Count:57
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Melting Point 71.0 °C
160 °F
ASTM D3417- ISO 3146
DuPont Elvax® CM576 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® CM576 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low ..
Melting Point 71.0 °C
160 °F
DuPont Fusabond® MC190D Ethylene Vinyl Acetate (28% VA)  (discontinued **)
Typical Use: Adhesion promoterCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideAvailability: North AmericaI..
Melting Point 71.0 °C
160 °F
DuPont Fusabond® MC250D Ethylene Vinyl Acetate (28% VA)  (discontinued **)
Typical Use: Adhesion promoterCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideAvailability: North AmericaI..
Melting Point 71.0 °C
160 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued
12 wt% Methacrylic Acid.Nucrel® 1214 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des..