Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 56.7 °C | 134 °F | ASTM D3418 |
LyondellBasell Lupolen® 5261 Z Q 456 B High Density Polyethylene, Pipe and Sheet Extrusion Grade Lupolen 5261 Z Q 456 B is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 um) p.. |
|||
Melting Point | 56.7 °C | 134 °F | ASTM D3418 |
LyondellBasell Lupolen® 5261 Z Q 456 High Density Polyethylene, Pipe and Sheet Extrusion Grade Lupolen 5261 Z Q 456 is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 µm) .. |
|||
Melting Point | 56.7 - 138 °C | 134 - 280 °F | Average value: 125 °C Grade Count:31 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |