LyondellBasell Lupolen® 5261 Z Q 456 High Density Polyethylene, Pipe and Sheet Extrusion Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Lupolen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Lupolen® 5261 Z Q 456 High Density Polyethylene, Pipe and Sheet Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lupolen 5261 Z Q 456 is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 µm) powder. It is not intended for medical or pharmaceutical applications. Processing Method: Extrusion Pipe, Sheet and Semi Finished Products. Physical Form: Powder. Typical Customer Applications: Plumbing, Heating and Cooling.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 28.3 MPa
4100 psi
2"/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2"/min; ASTM D638
Tensile Modulus 1.31 GPa
190 ksi
1% Secant; 0.5"/min; ASTM D638
Thermal Properties Metric English Comments
Melting Point 56.7 °C
134 °F
ASTM D3418
Vicat Softening Point 80.0 °C
176 °F
B/50 K/h 10N; ASTM D1525
130 °C
266 °F
A/50 K/h 10N; ASTM D1525