Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | <= -30.0 °C | <= -22.0 °F | |
M Chemical GUARD DOGâ„¢ UV123 HALS Light Stabilizer GUARD DOGâ„¢ UV123 hindered amine light stabilizer is highly effective in protecting polymers against degradation caused by exposure to UV radiation.Applications: GUARD DOGâ„¢ UV123 is mainly.. |
|||
Melting Point | -30.0 °C | -22.0 °F | Freezing Point |
LG Chemical TOTM Plasticizer Features: LG TOTM is used in cable and sheet by product that aging property and migration resistance among our products are superior.Application: Power cableInformation provided by LG Chemical |
|||
Melting Point | -30.0 °C | -22.0 °F | |
Solvay Chemicals 4_Ethoxy_1_1_1_trifluoro_3_buten_2_one Fluorinated Esters and Acetoacetates CAS-No.: 59938-06-6 / EC-No.: 475-900-3 Uses: Chemical intermediateInformation provided by Solvay |
|||
Melting Point | <= -30.0 °C | <= -22.0 °F | Freezing Point |
Solvay SIPOMER® SEM 25 Polyalkoxyl Polyarylphenol Ethylenic Methacrylate Description: Specialty monomer for Rheology modificationChemical Name: POLYALKOXYL POLYARYLPHENOL ETHYLENIC METHACRYLATECAS: 79-41-4Available in: Asia Pacific, Europe, Latin America and North Americ.. |
|||
Melting Point | -30.0 °C | -22.0 °F | Freezing Point |
Solvay Sulfuric Acid Electrolyte Grade Description: Sulfuric Acid electrolyte grade is colorless, clear and non-fuming with no visible sediment. It is very corrosive. The 93.2% strength solution complies with the Federal Specification O-.. |
|||
Melting Point | <= -30.0 °C | <= -22.0 °F | |
Dow Hydroxyethyl Acrylate Hydroxethyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow |
|||
Melting Point | -30.0 °C | -22.0 °F | |
BASF AMIX 100 Description: AMIX 1000 is a black, highly viscous liquid with an amine-like odor. It is miscible with water.Synonyms: Amin 1000, Diethylenetriamine residueApplications: Intermediate used in the pro.. |