Dow Hydroxyethyl Acrylate

Category Fluid
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Hydroxyethyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hydroxethyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow
Physical Properties Metric English Comments
Density 1.101 g/cc
0.03978 lb/in³
1.06 g/cc

@Temperature 66.0 °C
0.0383 lb/in³

@Temperature 151 °F
Viscosity 8.0 cP

@Temperature 15.5 °C
8.0 cP

@Temperature 59.9 °F
Molecular Weight 116.116 g/mol
116.116 g/mol
Maximum Moisture Content 0.15
0.15
wt% water
Vapor Pressure 0.000133 bar

@Temperature 25.0 °C
0.100 torr

@Temperature 77.0 °F
0.129 bar

@Temperature 135 °C
96.5 torr

@Temperature 275 °F
Thermal Properties Metric English Comments
Melting Point <= -30.0 °C
<= -22.0 °F
Boiling Point 192 °C
378 °F
760 mm Hg
Flammability Test 1.8
1.8
[mole %] Lower Flammability Limit @ 100°C
Flash Point 101.1 °C
214.0 °F
PMCC
Optical Properties Metric English Comments
Refractive Index 1.4481
1.4481
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm