Material Notes:
Fluorinated Esters and Acetoacetates CAS-No.: 59938-06-6 / EC-No.: 475-900-3 Uses: Chemical intermediateInformation provided by Solvay
Thermal Properties Metric English Comments
Melting Point -30.0 °C
-22.0 °F
Boiling Point 159 °C
318 °F
Flash Point 51.0 - 56.0 °C
124 - 133 °F
Flammable. (closed cup)
Descriptive Properties Value Comments
Appearance liquid
Color yellow
Composition >98%
Trans-4-ethoxy-1,1,1-trifluoro-3-buten-2-one