Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 468 °C | 874 °F | |
Schott BG7 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Transformation Temperature, Tg | 468 °C | 874 °F | |
Schott NG10 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG1, NG11, NG 12 |