Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 635 °C | 1180 °F | ISO 7884-8 |
Schott Glass 8436 Particularly resistant to sodium vapor and alkaline solutions, suitable to combinations with sapphire glass.Information provided by SCHOTT AG. |
|||
Transformation Temperature, Tg | 638 °C | 1180 °F | |
Schott N-LASF46A Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 636 °C | 1180 °F | |
Schott N-SK16 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 636 °C | 1180 °F | |
Schott N-LAK10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 639 °C | 1180 °F | |
Schott N-LAK21 Glass Information Provided by SCHOTT North America, Inc. |