Polymer Property : CTE, linear, Parallel to Flow = 8.33 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 - 15.0 µm/m-°C

@Temperature 50.0 - 150 °C
5.56 - 8.33 µin/in-°F

@Temperature 122 - 302 °F
ISO 11359-2
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
CTE, linear, Parallel to Flow 10.0 - 15.0 µm/m-°C

@Temperature 50.0 - 150 °C
5.56 - 8.33 µin/in-°F

@Temperature 122 - 302 °F
ISO 11359-2
Raschig Group DECAL® 937 Phenolic
Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W..
CTE, linear, Parallel to Flow 10.0 - 15.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
5.56 - 8.33 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)
Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade.
CTE, linear, Parallel to Flow 9.00 - 15.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
5.00 - 8.33 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® B 6550 LN PBT
Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF
CTE, linear, Parallel to Flow 10.0 - 15.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
5.56 - 8.33 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF