Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 9.00 µm/m-°C | 5.00 µin/in-°F | Below Tg; ISO 11359 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
CTE, linear, Parallel to Flow | 9.00 µm/m-°C | 5.00 µin/in-°F | Below Tg; ISO 11359 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
CTE, linear, Parallel to Flow | 9.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
5.00 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL34 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 9.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
5.00 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 9.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
5.00 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DC004E PC (Europe-Africa-Middle East) LNP* Thermocomp* DC004E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 9.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
5.00 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP LX03447 PEEK LNP* THERMOCOMP* LX03447 is a compound based on Polyetheretherketone containing Proprietary Filler(s). |
|||
CTE, linear, Parallel to Flow | 9.00 - 15.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
5.00 - 8.33 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |