Polymer Property : CTE, linear, Parallel to Flow = 58.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 58.0 µm/m-°C
32.2 µin/in-°F
ASTM D696
PolyOne Geon™ Vinyl Rigid Extrusion L0678 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
CTE, linear, Parallel to Flow 58.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
32.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
PolyOne Edgetek® TR2-30GF/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
CTE, linear, Parallel to Flow 58.0 µm/m-°C
32.2 µin/in-°F
ASTM D696
PolyOne Geon™ Vinyl Dry Blend E1354 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
CTE, linear, Parallel to Flow 58.0 µm/m-°C

@Temperature -30.0 - 100 °C
32.2 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1020 PP
SABIC® PPcompound 19T1020 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..
CTE, linear, Parallel to Flow 58.0 µm/m-°C

@Temperature -30.0 - 100 °C
32.2 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 9712 PP
SABIC® PPcompound 9712 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st..
CTE, linear, Parallel to Flow 58.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP WAL34I PBT (Europe-Africa-Middle East)
LNP* LUBRICOMP* WAL34I is a compound based on Polybutylene Terephalate resin containing PTFE, Aramid Fiber. Added features include Internally Lubricated.
CTE, linear, Parallel to Flow 58.0 µm/m-°C
32.2 µin/in-°F
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral
Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater..
CTE, linear, Parallel to Flow 58.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
32.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66
LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare.
CTE, linear, Parallel to Flow 58.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp RB008 PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RB008 is a compound based on PA 66 resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 58.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide RB008 PA66, 40% Glass Bead Filled, Injection Molded
Staramide RB008 is a 40% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 58.0 µm/m-°C

@Temperature -30.0 - 100 °C
32.2 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP
SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications...