Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 400 µm/m-°C @Temperature 23.0 - 80.0 °C |
222 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded AG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 400 µm/m-°C @Temperature 23.0 - 80.0 °C |
222 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
Eurostar Staramide AG6ST43H PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG6ST43H is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 400 µm/m-°C @Temperature 23.0 - 80.0 °C |
222 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
Eurostar Staramide AK6 PA66, 30% Mineral Reinforced, Injection Molding Staramide AK6 is a 30% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |