Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Eurostar Engineering Plastics
Trade Name Staramide
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
on Tensile Bar; ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
5 mm/min; ISO 527
Elongation at Break 5.0 %
5.0 %
5 mm/min; ISO 527
Tensile Modulus 5.80 GPa
841 ksi
1 mm/min; ISO 527
Izod Impact, Notched (ISO) 16.0 kJ/m²

@Temperature -40.0 °C
7.61 ft-lb/in²

@Temperature -40.0 °F
Edgew 80x10x4; ISO 180/1A
18.0 kJ/m²

@Temperature -20.0 °C
8.57 ft-lb/in²

@Temperature -4.00 °F
Edgew 80x10x4; ISO 180/1A
22.0 kJ/m²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 400 µm/m-°C

@Temperature 23.0 - 80.0 °C
222 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Af
Vicat Softening Point 250 °C
482 °F
B/120; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Zone 1
Middle Barrel Temperature 270 - 280 °C
518 - 536 °F
Zone 2
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Zone 3
Melt Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 75.0 - 85.0 °C
167 - 185 °F
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Moisture Content 0.20 %
0.20 %
Copyright © lookpolymers.com All Rights Reserved