Polymer Property : CTE, linear, Parallel to Flow = 222 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 400 µm/m-°C

@Temperature 23.0 - 80.0 °C
222 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded
AG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
CTE, linear, Parallel to Flow 400 µm/m-°C

@Temperature 23.0 - 80.0 °C
222 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Eurostar Staramide AG6ST43H PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding
Staramide AG6ST43H is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 400 µm/m-°C

@Temperature 23.0 - 80.0 °C
222 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Eurostar Staramide AK6 PA66, 30% Mineral Reinforced, Injection Molding
Staramide AK6 is a 30% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.