Polymer Property : CTE, linear, Parallel to Flow = 30.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 55.0 µm/m-°C
30.6 µin/in-°F
ASTM D696
LG Chemical LUMID HI3232A(W) PA6+MF23%, High Impact
Feature: Injection Molding, PA6+MF23%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 14807-96-6Information provided by LG Chemical
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 23.0 - 150 °C
30.6 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM CRS5011 PEI (Europe-Africa-Middle East)
Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
30.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 815UX PBT (Europe-Africa-Middle East)
VALOX 815UX is a 15% glass reinforced PBT+PET blend with improved surface appearance and excellent UV performance.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
30.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East)
VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a..
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 23.0 - 150 °C
30.6 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 9076 PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
30.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS
LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable.
CTE, linear, Parallel to Flow 55.0 µm/m-°C
30.6 µin/in-°F
ISO 11359-1/-2
Covestro Bayblend® ET 1100* Polycarbonate + ABS, Mineral Filled
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
CTE, linear, Parallel to Flow 55.0 µm/m-°C
30.6 µin/in-°F
ISO 11359-1/-2
Covestro Bayblend® T95 MF* Polycarbonate + ABS, Mineral Filled
Developmental productInjection molding grade9 % mineral filledvery high heat resistancereduced coefficient of linear thermal expansiontensile modulus = 3350 MPaVicat/B 120 = 142 °CPreprocessingMax...
CTE, linear, Parallel to Flow 55.0 µm/m-°C
30.6 µin/in-°F
dry; ISO 11359-1/-2
DSM EcoPaXX® Q-PG6 PA410-I-GF30
% Glass Reinforced, Impact Modified
CTE, linear, Parallel to Flow 55.0 µm/m-°C
30.6 µin/in-°F
dry; ISO 11359-1/-2
DSM EcoPaXX® Q-X07208 PA410-I-GF30
% Glass Reinforced, Impact Modified
CTE, linear, Parallel to Flow 55.0 µm/m-°C
30.6 µin/in-°F
ISO 11359-1/-2
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled
MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa..
CTE, linear, Parallel to Flow 55.0 µm/m-°C
30.6 µin/in-°F
ISO 11359-1/-2
Covestro Makrolon® SF800Z Polycarbonate, 5% Glass Filled
MVR (300 °C/1.2 kg) 8.0 cm3/10 minStructural foam5 % Glass fiber reinforcedMilled fiberChlorine- and bromine-free flame retardantMedium viscosityEasy releaseInjection moldingAvailable in natural (o..
CTE, linear, Parallel to Flow 55.0 µm/m-°C
30.6 µin/in-°F
ISO 11359-1/-2
Barlog Plastics KEBATER BFA15 PBT, 15% glass fiber reinforced, flame retardant
PBT-GF15 FRInformation provided by BARLOG plastics GmbH.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
BASF Procom® C40H 451 Polypropylene
Used for: instrument panels, motor vehicle grills, heater boxes.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
BASF Procom® C40H 455 Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
BASF Procom® C40H 458 Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
BASF Procom® D 1012 Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
BASF Procom® D 1173 Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
BASF Luranyl® KR 2403 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced
General-purpose grade with 10% glass fiber for parts requiring especially good resistance to heat deformation.Applications: auto parts, steering-column cladding and water meters.Data was collected b..
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
BASF Procom® T40H 550 Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
BASF Procom® T40H 564 Polypropylene
Car heater casings.Data was collected by ISO methods and provided by BASF.