Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 55.0 µm/m-°C | 30.6 µin/in-°F | ASTM D696 |
LG Chemical LUMID HI3232A(W) PA6+MF23%, High Impact Feature: Injection Molding, PA6+MF23%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Europe-Africa-Middle East) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
30.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 815UX PBT (Europe-Africa-Middle East) VALOX 815UX is a 15% glass reinforced PBT+PET blend with improved surface appearance and excellent UV performance. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
30.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East) VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 9076 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
30.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C | 30.6 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® ET 1100* Polycarbonate + ABS, Mineral Filled As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C | 30.6 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® T95 MF* Polycarbonate + ABS, Mineral Filled Developmental productInjection molding grade9 % mineral filledvery high heat resistancereduced coefficient of linear thermal expansiontensile modulus = 3350 MPaVicat/B 120 = 142 °CPreprocessingMax... |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C | 30.6 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-PG6 PA410-I-GF30 % Glass Reinforced, Impact Modified |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C | 30.6 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-X07208 PA410-I-GF30 % Glass Reinforced, Impact Modified |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C | 30.6 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C | 30.6 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® SF800Z Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 8.0 cm3/10 minStructural foam5 % Glass fiber reinforcedMilled fiberChlorine- and bromine-free flame retardantMedium viscosityEasy releaseInjection moldingAvailable in natural (o.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C | 30.6 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATER BFA15 PBT, 15% glass fiber reinforced, flame retardant PBT-GF15 FRInformation provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® C40H 451 Polypropylene Used for: instrument panels, motor vehicle grills, heater boxes.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® C40H 455 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® C40H 458 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® D 1012 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® D 1173 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Luranyl® KR 2403 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced General-purpose grade with 10% glass fiber for parts requiring especially good resistance to heat deformation.Applications: auto parts, steering-column cladding and water meters.Data was collected b.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® T40H 550 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® T40H 564 Polypropylene Car heater casings.Data was collected by ISO methods and provided by BASF. |