Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ASTM D696 |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Pocan® ECO T 3215 000000 PBT + PET, 15% Glass Fiber PBT + PET, 15% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 1000FC PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. NSF-51 certified for selected colors. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 1010X PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with low ionic contamination of less than 0.1 ppm each of leachable chloride and sulphates. ECO Conforming. Factory Mutual FM4910 compliant in recognized color.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 1100R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), .. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
27.8 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK) KetaSpire® KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standard.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
27.8 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers Ryton® QC200P Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GFN1V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1V is a 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP 7665 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnite® TV8 260 PBT-30% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® AS/2 PA66 Product description: Grilon AS/2 is an unreinforced PA66 injection molding grade. Grilon AS/2 has the following important properties: Good flow behaviorEasy processingShort cycle times Grilon AS/2 i.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-15 PA6-GF15 Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-3 ESD PA12-GF30 Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced PBT-GF10Information provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® D 1158 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® D 1189 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be sup.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM AUT200 PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperatu.. |