Polymer Property : Heat of Fusion = 45.0 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 34.0 - 45.0 J/g
14.6 - 19.4 BTU/lb
DSC
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)  (discontinued **)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis..
Heat of Fusion 35.0 - 45.0 J/g
15.1 - 19.4 BTU/lb
Crystallization Heat; DSC
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)  (discontinued **)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis..
Heat of Fusion 35.0 - 45.0 J/g
15.1 - 19.4 BTU/lb
Crystallization Heat; DSC
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis..
Heat of Fusion 35.0 - 45.0 J/g
15.1 - 19.4 BTU/lb
DSC
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis..