Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 35.0 - 45.0 J/g | 15.1 - 19.4 BTU/lb | Crystallization Heat; DSC |
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)
(discontinued **) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Heat of Fusion | 35.0 - 45.0 J/g | 15.1 - 19.4 BTU/lb | Crystallization Heat; DSC |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Heat of Fusion | 35.0 - 45.0 J/g | 15.1 - 19.4 BTU/lb | DSC |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Heat of Fusion | 35.0 - 40.0 J/g | 15.1 - 17.2 BTU/lb | ASTM D3417 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |