Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | flat, curved or corrugated surfaces with rivets |
3M Controltac™ IJ181 Graphic Film 2-mil white, vinyl film; Specifically formulated for use on stainless steel; Pressure-activated adhesive for easy sliding, tacking, snap-up and repositioning; Flexible, conforms to moderate curves, .. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M FP019808 White Polyester Label Products 3M™ White Polypropylene Label Products FP019802 and FP019808 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is for labeling tires when u.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M FP024900 White Polypropylene Label Products 3M™ White Polypropylene Label Products are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M FP026508 White Polyester Label Products 3M™ White Polypropylene Label Products FP017102 and FP026508 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general purpose permane.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M FV052 Tire Vinyl Label Products 3M™ Tire Vinyl Label Products are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling tires when used w.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M FV052R Tire Vinyl Label Products 3M™ Tire Vinyl Label Products are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling tires when used w.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M FV053 Tire Vinyl Label Products 3M™ Tire Vinyl Label Products are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling tires when used w.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M FV855 Tire Vinyl Label Products 3M™ Tire Vinyl Label Products FV852 and FV855 are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling t.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M PS192 White Yupo™ TIS Label Products 3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M PS197 White Yupo™ TIS Label Products 3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Air and substrate, for flat surfaces with rivets |
3M Scotchcal™ 5000 Reflective Graphic Film' 6-mil, enclosed lens, retroflective, flexible films; Pressure-sensitive adhesive; Permanent; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity w.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Dry; flat, curved or corrugated surfaces with rivets |
3M Scotchlite™ 5100 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Permanent; Available in 15 colors, including black (which reflects whit.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Air and substrates, for flat surfaces with rivets |
3M Scotchlite™ 5100 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Permanent; Available in 15 colors, including black (which reflects whit.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Air and substrates, for flat surfaces with rivets |
3M Scotchlite™ 5100-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Permanent; Available in 15 colors, including black (which reflects whit.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Air and substrates, for flat surfaces with rivets |
3M Scotchlite™ 5100R Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Removable with heat; Available in 15 colors, including black (which ref.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | flat surfaces without rivets |
3M Scotchlite™ 680-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | flat surfaces without rivets |
3M Scotchlite™ 680-14 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | flat surfaces without rivets |
3M Scotchlite™ 680-71 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | flat surfaces without rivets |
3M Scotchlite™ 680-75 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | flat surfaces without rivets |
3M Scotchlite™ 680-77 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | flat surfaces without rivets |
3M Scotchlite™ 680-81 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Dry; flat, curved or corrugated surfaces with rivets |
3M Scotchlite™ IJ5100-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Permanent; Available in 15 colors, including black (which reflects whit.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | flat, curved or corrugated surfaces with rivets |
3M Scotchlite™ IJ680-10 Reflective Graphic Film 6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Air and substrates, for flat surfaces with rivets |
3M Scotchlite™ RG5100R-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Removable with heat; Available in 15 colors, including black (which ref.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | flat, curved or corrugated surfaces with rivets |
3M Scotchlite™ RG680-10 Reflective Graphic Film 6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M FM482 Clear Polyester Label Product 3M™ Clear Polyester Label Product FM482 is a durable, high performance material that offers thermal stability and moisture resistance. This polyester label product utilizes 3M™ Adhesive P1110, whi.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M FM532 White Polyester Label Products 3M™ White Polyester Label Products FM53R2, FM532 and FM782 are durable, high performance materials that utilize 3M™ Adhesive P1110, which is for labeling tires when used with tire wash. This adhes.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Application |
3M PS102 Semi-gloss Paper Label Product 3M™ Semi-gloss Paper Label Product PS102 is a durable, general purpose paper product. This label product utilizes 3M™ Adhesive P1110, which is for labeling tires when used with tire wash. This adh.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Dry; flat, curved or corrugated surfaces with rivets |
3M Scotchlite™ IJ5100R-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Removable with heat; Available in 15 colors, including black (which ref.. |
|||
Minimum Service Temperature, Air | 13.0 °C | 55.4 °F | Air and substrates, for flat surfaces with rivets |
3M Scotchlite™ IJ5100R-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Removable with heat; Available in 15 colors, including black (which ref.. |