3M PS102 Semi-gloss Paper Label Product

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M PS102 Semi-gloss Paper Label Product.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Semi-gloss Paper Label Product PS102 is a durable, general purpose paper product. This label product utilizes 3M™ Adhesive P1110, which is for labeling tires when used with tire wash. This adhesive exhibits high initial tack, yet resists edge bleed and cold flow.Information provided by 3M
Physical Properties Metric English Comments
Thickness 78.7 microns
3.10 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.701 kN/m
4.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 43.0 °C
109 °F
Application
68.0 °C
154 °F
Service
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Service
13.0 °C
55.4 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type P1110 Perm 26
Liner 50# SC