Material Notes:
2-mil white, vinyl film; Specifically formulated for use on stainless steel; Pressure-activated adhesive for easy sliding, tacking, snap-up and repositioning; Flexible, conforms to moderate curves, corrugations and rivets; Permanent filmInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
76.2 - 102 microns
3.00 - 4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.2 MPa
2490 psi
Peel Strength 1.05 kN/m
6.00 pli
Adhesion to Stainless steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
flat surfaces without rivets
38.0 °C
100 °F
flat, curved or corrugated surfaces with rivets
Minimum Service Temperature, Air 10.0 °C
50.0 °F
flat surfaces without rivets
13.0 °C
55.4 °F
flat, curved or corrugated surfaces with rivets