Thermal Properties Metric English Comments
Minimum Service Temperature, Air -42.0 °C
-43.6 °F
P & P Technology A320C UL Neoprene/EPDM
SAE J18 Specification: 2C2 ASTM Specification: 2C2 (1985&91). SCE42 (1967&68). RE42E1 (1978)Flame Resistance: Pass UL94V-0, HBF, HF-1**, GM609OMB4,A FMVSS302 Pass @ 0.8mm.IMDS Node ID: 13900758Infor..
Minimum Service Temperature, Air -42.0 °C
-43.6 °F
Gehman T100
Zeon Chemicals HyTemp® 4053EP AR Polyacrylate Elastomer
HyTemp 4053EP contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent low temperature, oil, heat and compression set resistance.Excellent..
Minimum Service Temperature, Air -42.0 °C
-43.6 °F
DuPont Test Method
DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer
Kalrez® Spectrum™ 0040 perfluoroelastomer parts are specifically designed for low-temperature environments where significant chemical resistance is required. Proprietary polymer and cure technolog..