P & P Technology A320C UL Neoprene/EPDM

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer P & P Technology
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology A320C UL Neoprene/EPDM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SAE J18 Specification: 2C2 ASTM Specification: 2C2 (1985&91). SCE42 (1967&68). RE42E1 (1978)Flame Resistance: Pass UL94V-0, HBF, HF-1**, GM609OMB4,A FMVSS302 Pass @ 0.8mm.IMDS Node ID: 13900758Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 0.0864 - 0.1056 g/cc
0.0864 - 0.1056 g/cc
Water Absorption <= 0.050 %
<= 0.050 %
0.10 %
0.10 %
Allowed
Deformation 25 %

@Pressure 0.00345 - 0.0621 MPa
25 %

@Pressure 0.500 - 9.01 psi
Mechanical Properties Metric English Comments
Hardness, Shore OO 50
50
Tensile Strength >= 0.827 MPa
>= 120 psi
Elongation at Break >= 150 %
>= 150 %
Compression Set <= 12.5 %
<= 12.5 %
D3575; 0.5
<= 25 %
<= 25 %
D1056; 0.5
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -42.0 °C
-43.6 °F
Flammability, UL94 V-0
V-0
Shrinkage <= 5.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %

@Temperature 158 °F,
Time 168 hour
Heat Ageing Lineal
Descriptive Properties Value Comments
Fluid Immersion <250%
ASTM E, Fuel B
Heat Ageing Max Change 305
7 days @ 70°C
Ozone Resistance Rating 0'
72 hrs @ 50pphm, ASTM D1171