Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Kalrez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Kalrez® Spectrum™ 0040 perfluoroelastomer parts are specifically designed for low-temperature environments where significant chemical resistance is required. Proprietary polymer and cure technology promotes low-temperature sealing performance (-42°C) of Kalrez® Spectrum™ 0040 parts to temperatures typically unattainable for perfluoroelastomers parts. Kalrez® Spectrum™ 0040 is an excellent choice in applications such as couplings for the chemical transportation industry, or for other applications where chemical resistance and elasticity are required in some of the coldest environments. The volume swell for Kalrez® Spectrum™ 0040 is approximately 10% when exposed to nitric acid at 110°C for 168 hours. Compression set resistance is similar to that of our broad chemically-resistant product, Kalrez® Spectrum™ 6375.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Elongation at Break 170 %
170 %
ASTM D412
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D412
Compression Set 41 %

@Temperature 200 °C,
Time 252000 sec
41 %

@Temperature 392 °F,
Time 70.0 hour
ASTM D395B
57 %

@Temperature 200 °C,
Time 1.21e+6 sec
57 %

@Temperature 392 °F,
Time 336 hour
ASTM D395B
62 %

@Temperature 200 °C,
Time 2.42e+6 sec
62 %

@Temperature 392 °F,
Time 672 hour
ASTM D395B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
DuPont Test Method
Minimum Service Temperature, Air -42.0 °C
-43.6 °F
DuPont Test Method
-17.0 °C
1.40 °F
Retraction Temperature, Tr10; ASTM D1329
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
DuPont Test Method
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: