Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -270 - -79.0 °C | -454 - -110 °F | Average value: -183 °C Grade Count:26 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |