Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -15.5 °C | 4.10 °F | Gehman torsion test, T10 |
Daikin DAI-EL G-702 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent elongation and tear strength.Informatio.. |
|||
Minimum Service Temperature, Air | -15.5 °C | 4.10 °F | Gehman torsion test, T10 |
Daikin DAI-EL G-723 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability, non-sticking.Information provided by Dai.. |
|||
Minimum Service Temperature, Air | -15.5 °C | 4.10 °F | Gehman torsion test, T10 |
Daikin DAI-EL G-755 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Extrusion of hose and tubing, etc.Information provided by Daikin Indus.. |
|||
Minimum Service Temperature, Air | -15.5 °C | 4.10 °F | Gehman torsion test, T10 |
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries. |