ExxonMobil PP1055E2 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP1055E2 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A nucleated homopolymer resin with good flowability and antistatic properties. It is designed for molding of media packaging, containers and other articles requiring fast molding cycles.Availability: Africa & Middle East and Europe Features:AntistaticFast Molding CycleNucleatedUses: CapsClosuresConsumer ApplicationsContainersLidsRigid PackagingProcessing Method: Injection Molding and CompoundingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 53 g/10 min

@Load 2.16 kg,
Temperature 230 °C
53 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
ISO 868
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527-2/50
Elongation at Yield 8.0 %
8.0 %
ISO 527-2/50
Tensile Modulus 1.65 GPa
239 ksi
ISO527-2/1
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched (ISO) 1.49 kJ/m²
0.710 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.199 J/cm²
0.950 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 324 °C
615 °F
ISO 3146
Crystallization Temperature 253 °C
487 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 56.1 °C
133 °F
ISO 75-2/A
Vicat Softening Point 153 °C
307 °F
ISO 306/A50