Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 110 °C | 230 °F | ExxonMobil Method |
ExxonMobil LL 1235x70 Cast Film Resin
(discontinued **) LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Crystallization Temperature | 110 °C | 230 °F | ASTM D3418 |
Ineos H03W-01 Polypropylene, Gas Phase Polymerized H03W-01 (formerly Fortilene® HG3253) belongs to the new generation of polypropylenes produced by gas phase polymerization. This nominal 4 melt flow index product is specifically designed for fib.. |
|||
Crystallization Temperature | 110 °C | 230 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M3204 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-surf.. |
|||
Crystallization Temperature | 110 °C | 230 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M40 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-su.. |
|||
Crystallization Temperature | 110 °C | 230 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M70 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cyc.. |
|||
Crystallization Temperature | 110 °C | 230 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M735 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cycle.. |