Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 133 °C | 271 °F | Melting; DSC |
LG Chemical LUTENE-H FE0070 HDPE LUTENE-H FE0070 is mainly intended for the extrusion of blown film with high mechanical properties for the manufacture of "T-Shirt" grocery sacks, can liners. Especially, LUTENE-H FE0070 resin can b.. |
|||
Crystallization Temperature | 133 °C | 271 °F | Melting; DSC |
LG Chemical SEETEC PB150 HDPE Features: This high molecular weight, hexane copolymer is tailored for high impact blow-molded containers that require:Excellent processabilityHigh impact strength at low temperatureOutstanding stre.. |
|||
Crystallization Temperature | 133 - 140 °C | 271 - 284 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Ajedium™ PVDF 9009 Polyvinylidene Fluoride (PVDF) Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea.. |
|||
Crystallization Temperature | 133 - 138 °C | 271 - 280 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Crystallization Temperature | 133 - 140 °C | 271 - 284 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53... |
|||
Crystallization Temperature | 133 - 138 °C | 271 - 280 °F | Peak, DSC; ASTM D3418 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Crystallization Temperature | 133 - 140 °C | 271 - 284 °F | Peak, DSC; ASTM D3418 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Crystallization Temperature | 133 - 140 °C | 271 - 284 °F | Peak, DSC; ASTM D3418 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Crystallization Temperature | 133 °C | 271 °F | Melting; DSC |
LG Chemical LUTENE-H ME9180 HDPE Description: LUTENE-H ME9180 is mainly intended for injection molding of complicated parts. It has high productivity and good appearance.Applications: Complicated parts, light-weight household.CAS N.. |