LG Chemical SEETEC PB150 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer LG Chemical
Trade Name SEETEC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC PB150 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: This high molecular weight, hexane copolymer is tailored for high impact blow-molded containers that require:Excellent processabilityHigh impact strength at low temperatureOutstanding stress crack resistance (ESCR)Good melt strengthApplications: Fuel Tank, IBC, Jerry can, Agri-chemical containerCAS No. 25213-02-9Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.944 - 0.947 g/cc
0.944 - 0.947 g/cc
ASTM D1505
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50; ASTM D1693
Melt Flow 5.4 - 6.6 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.4 - 6.6 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.5 MPa
3410 psi
50 mm/min; ASTM D638
Elongation at Break >= 600 %

@Thickness 50.0 mm
>= 600 %

@Thickness 1.97 in
ASTM D638
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Izod Impact, Unnotched >= NB

@Temperature 23.0 °C
>= NB

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
10°C/min; ASTM D3418
Crystallization Temperature 133 °C
271 °F
Melting; DSC
Vicat Softening Point 125 °C
257 °F
ASTM D1525