Polymer Property : Vicat Softening Point = 385 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 196 °C
385 °F
49 N; ISO 306, ASTM D1525
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex..
Vicat Softening Point 196 °C
385 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Vicat Softening Point 196 °C
385 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East)
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Vicat Softening Point 196 °C
385 °F
B 120; ISO 306
Ter Hell Plastic Terez® PA 6 7750 TK Polyamide 6
Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information pr..
Vicat Softening Point 196 °C
385 °F
B/50; ISO 306
Ter Hell Plastic Terez® PA 6 7751 TGF 15 GL Polyamide 6, 15% Glass Fiber
Description: Medium viscosity, dry impact resistant PA 6, 15% glass fiber reinforced and improved surface gloss.Application: For molding parts with good stiffness and high dimensional stability.In..
Vicat Softening Point 196 - 215 °C
385 - 419 °F
Average value: 203 °C Grade Count:5
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..